Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 2880 min | 48.0 hour | Full Cure |
Parker Chomerics CHO-FORM 5537 EMI Shielding Material Fast Curing Form-in-Place EMI Shielding Material. Cho-Form 5537 is a one component, moisture cured, electrically conductive, form-in-place EMI gasketing material. The formulation contains nickel-pla.. |
|||
Cure Time | 2880 min @Temperature 23.0 °C |
48.0 hour @Temperature 73.4 °F |
50% RH |
Parker Chomerics THERM-A-FORM 1641 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 2880 min @Temperature 25.0 °C |
48.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond 216R02 Quick Set Electrical Insulator TRA-BOND 216R02 is an exceptional epoxy formulation recommended for applications where both quick set-up and a low-viscosity material are required. This clear, two-part, low-viscosity system is easi.. |
|||
Cure Time | 2880 min | 48.0 hour | 85% maximum strength developed within |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
Cure Time | 2880 min @Temperature 25.0 °C |
48.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond FS12 Fast Cure Epoxy Adhesive System TRA-BOND FS12 is an epoxy resin formulation developed for room temperature bonding applications where a fast cure epoxy adhesive is needed. This effective epoxy formulation consists of 100% reactive.. |
|||
Cure Time | 2880 min @Temperature 22.0 °C |
48.0 hour @Temperature 71.6 °F |
|
Dow Corning HM-2500 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Cure Time | 2880 min @Temperature 22.0 °C |
48.0 hour @Temperature 71.6 °F |
|
Dow Corning HM-2510 CLEAR ASSEMBLY SEALANT A reactive Hot Melt silicone sealant that has immediate strength and crosslinks into a neutral cure RTV sealantInformation provided by Dow Corning |
|||
Cure Time | 2880 min @Temperature 22.0 °C |
48.0 hour @Temperature 71.6 °F |
|
Dow Corning SE 9184 WHITE RTV One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning |
|||
Cure Time | 2880 min | 48.0 hour | |
3M AC-215 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M AC-236 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M AC-236 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M AC-275 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst.. |
|||
Cure Time | 2880 min | 48.0 hour | Tack-Free Time |
3M AC-350 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M AC-350 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are.. |
|||
Cure Time | 2880 min | 48.0 hour | Tack-Free Time |
3M AC-665 Class C-24 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Cure Time | 2880 min | 48.0 hour | Tack-Free Time |
3M AC-730 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Cure Time | 2880 min | 48.0 hour | Full Cure |
3M Scotch-Weld™ DP620NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-620NS is a back, long working time, two-component polyurethane. Formulated as 1:1 ratio liquids. With the squeeze of the trigger, or with automated dispensing.. |
|||
Cure Time | 2880 min | 48.0 hour | Full Cure |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Cure Time | >= 2880 min @Temperature 24.0 °C |
>= 48.0 hour @Temperature 75.2 °F |
|
BCC Products BC 7062-3H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |
|||
Cure Time | 2880 min | 48.0 hour | |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Cure Time | 2880 - 4320 min | 48.0 - 72.0 hour | ambient temperatures |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |
|||
Cure Time | 2880 min | 48.0 hour | Tack-Free Time |
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |