Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SE 9184 WHITE RTV

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Dow Corning SE 9184 WHITE RTV.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
One-part, white, moisture cure RTV, non-flowing, fast tack free, controlled volatility, thermally conductive, UL V-0.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 2.22 g/cc

@Temperature 25.0 °C
2.22 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Ultimate 2.90 MPa
420 psi
Elongation at Break 70 %
70 %
Shear Strength 2.07 MPa
300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
Dielectric Strength 19.7 kV/mm
500 kV/in
Processing Properties Metric English Comments
Cure Time 2880 min

@Temperature 22.0 °C
48.0 hour

@Temperature 71.6 °F
Shelf Life 7.00 Month
7.00 Month
Descriptive Properties Value Comments
Color white
Flowable yes
Water Resistant yes
Users viewing this material also viewed the following: