Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Screw Speed | 30 - 90 rpm | 30 - 90 rpm | |
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Screw Speed | 60 - 90 rpm | 60 - 90 rpm | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Screw Speed | 60 - 90 rpm | 60 - 90 rpm | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |