Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP514-447 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9902 Very Dark Gray Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 149 psi | |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Typically 50 psi |
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Back Pressure | >= 0.345 MPa | >= 50.0 psi | no units given |
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Star Plastics PC731 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.345 - 1.38 MPa | 50.0 - 200 psi | |
Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.345 MPa | 50.0 psi | |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
Clariant Renol 6602-L Nylon 66, Internally Lubricated Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® SMU5835 Polyetherimide, 25% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |