Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ALPHALAC SH860 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical KEYFLEX TO1192A Olefin Type TPE Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP1007F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL GP3202B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HG3100 PP+MF10%, High Gloss Description: Injection Molding, PP+MF10%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical SG175 ABS, Super Surface Gloss Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HI5204B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HM2300 PP+GF30% Description: Injection Molding, PP+GF30%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HM3102A PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HM5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL HR2100D PP+GF17% Description: Injection Molding, PP+GF17%, General PurposeApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 165997-17-3Information provided by LG Chemical |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |