Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 1.03 MPa | 0.000 - 149 psi | |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Back Pressure | 0.000 - 0.827 MPa | 0.000 - 120 psi | |
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non.. |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.000 - 0.827 MPa | 0.000 - 120 psi | |
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Back Pressure | 0.000 - 0.827 MPa | 0.000 - 120 psi | |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Back Pressure | 0.000 - 0.827 MPa | 0.000 - 120 psi | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Back Pressure | 0.000 - 1.96 MPa | 0.000 - 284 psi | Injection Molding |
LG Chemical LUCON CP6062EX PC/ABS+CNT Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface ResistivityApplication: BLU Carrying TrayCAS No. 103598-77-2, 9003-56-9, .. |
|||
Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Back Pressure | 0.000 - 0.172 MPa | 0.000 - 25.0 psi | Injection Molding |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |
|||
Back Pressure | 0.000 - 0.517 MPa | 0.000 - 75.0 psi | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Back Pressure | 0.000 - 10.0 MPa | 0.000 - 1450 psi | |
Kingfa MAC-451PG Electroplating PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor.. |
|||
Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled Data provided by Clariant Masterbatches |