Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical LUPOL HI5205R PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM; Dehumidified Dryer |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Eurotec® Tecotek® PC44 GR003 ZG70 PC, unfilled, flame retardant - halogen (RoHS compliant), light grey Information provided by Eurotec® |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Extrusion Molding |
LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly.. |