Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 98.9 - 104 °C | 210 - 220 °F | |
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 98.9 - 104 °C | 210 - 220 °F | |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Drying Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Edgetek® PS-15GF-25MN/000 Polybutylene Terephthalate (PBT), Glass/Mineral Filled
(discontinued **)< Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 82.2 - 104 °C | 180 - 220 °F | |
PolyOne Lubri-Tech™ PS-30GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Lubri-Tech™ NI-30CF/10T-2S Nylon 6/10, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(discontinue Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 87.8 - 104 °C | 190 - 220 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.2 - 104 °C | 180 - 220 °F | |
PolyOne Lubri-Tech™ PS-30GF/10T2S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(d Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |