Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 °C | 248 °F | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Drying Temperature | 120 - 130 °C | 248 - 266 °F | |
PolyOne Stat-Tech™ PC-08CF/000 FR V0 Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Drying Temperature | 120 °C | 248 °F | |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Drying Temperature | 120 °C | 248 °F | overnight before use |
Victrex® Vicote® F806 Polyetheretherketone (PEEK) Liquid Dispersion The VICOTE F805 natural, F806 natural and F807Blk grades have been specifically formulated to provide a tough, resilient, high wear resistant coating with varying levels of lubricants on ferrous and.. |
|||
Drying Temperature | 120 °C | 248 °F | |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Drying Temperature | 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
|
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 120 °C | 248 °F | Injection Molding |
LG Chemical Lupox® TE5011M PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA), 50% Glass Fiber Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
|
Solvay Specialty Polymers Amodel® FC -1160 Polyphthalamide (PPA), 60% Glass Fiber Amodel® FC-1160 is an FDA-approved, 60% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Drying Temperature | 120 °C @Time 1800 - 5400 sec |
248 °F @Time 0.500 - 1.50 hour |
|
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Drying Temperature | 120 °C @Time 16200 sec |
248 °F @Time 4.50 hour |
|
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Drying Temperature | 120 °C | 248 °F | |
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Drying Temperature | 120 - 130 °C | 248 - 266 °F | Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens. |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/50-20T PEEK, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Drying Temperature | 120 °C | 248 °F | |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |
|||
Drying Temperature | 120 - 150 °C @Time 10800 sec |
248 - 302 °F @Time 3.00 hour |
|
LATI Latilub 88/10-10T Y/10 PEEK, 10% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |