Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 110 - 130 °C | 230 - 266 °F | |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Drying Temperature | 90.0 - 130 °C | 194 - 266 °F | Average value: 108 °C Grade Count:27 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Drying Temperature | 120 - 130 °C | 248 - 266 °F | Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens. |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Latilon 28D PC Polycarbonate (PC). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability. Very good surface appearanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Drying Temperature | 110 - 130 °C | 230 - 266 °F | |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Drying Temperature | 110 - 130 °C @Time 10800 sec |
230 - 266 °F @Time 3.00 hour |
|
LATI Latilub 95-15T PSU, PTFE Filled Self-lubricating product based on Polysulfone (PSU). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici .. |
|||
Drying Temperature | 80.0 - 130 °C | 176 - 266 °F | Average value: 108 °C Grade Count:31 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |
|||
Drying Temperature | 120 - 130 °C @Time 10800 sec |
248 - 266 °F @Time 3.00 hour |
|
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Drying Temperature | 110 - 130 °C | 230 - 266 °F | Injection Molding |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |