Polymer Property : Rear Barrel Temperature = 285 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 263 - 285 °C
505 - 545 °F
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced
Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Rear Barrel Temperature 263 - 285 °C
505 - 545 °F
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced
Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Rear Barrel Temperature 263 - 285 °C
505 - 545 °F
Polymer Resources PC/TP-GP2-G20 PC Polyester, Excellent Chemical Resistance, 20% Glass Filled  (Unverified
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 275 - 285 °C
527 - 545 °F
Injection Molding
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID LW4303B(W) PA66+MF30%, Low Warpage
Feature: Injection Molding, PA66+MF30%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage
Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information ..
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro..
Rear Barrel Temperature 270 - 285 °C
518 - 545 °F
Injection Molding
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact
Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov..
Rear Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 1
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Rear Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 1
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
Rear Barrel Temperature 275 - 285 °C
527 - 545 °F
Zone 1
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..