Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 135 - 163 °C | 275 - 325 °F | |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Mold Temperature | 135 - 163 °C | 275 - 325 °F | |
LNP Stat-Kon® LCL-4026 EM BK8-115 Polyetheretherketone, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(d Features: Electrically Conductive, Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discont.. |
|||
Mold Temperature | 121 - 163 °C | 250 - 325 °F | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Mold Temperature | 107 - 163 °C | 225 - 325 °F | |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Mold Temperature | 121 - 163 °C | 250 - 325 °F | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Mold Temperature | 135 - 163 °C | 275 - 325 °F | |
Clariant Renol PPA1100G60 Polyphthalamide, 60% Glass Fiber Data provided by Clariant Masterbatches |