Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Mold Temperature | 65.6 - 104 °C | 150 - 220 °F | |
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |