Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 140 - 160 °C | 284 - 320 °F | |
PolyOne Edgetek® ES-30GF/000 Black Polyethersulfone (PESU) Edgetek™ ES-30GF/000 Black XP120031Information provided by PolyOne |
|||
Mold Temperature | 140 - 165 °C | 284 - 329 °F | |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ Electro 242-1 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ Electro 242-2 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ FFSL 7041 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6050 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LIM 6071 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2080 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2540 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2670 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 3786/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4020 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR TOPCOAT 3719 Liquid Silicone Rubber Specialty Coating Low Surface Friction Coating / USP Class VI Compliancy - Physical Properties are subject to the substrate that is used. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Siloprenâ„¢ LSR 4080 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Mold Temperature | 140 - 160 °C | 284 - 320 °F | DAM |
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA) Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also.. |
|||
Mold Temperature | 140 - 165 °C | 284 - 329 °F | |
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
Mold Temperature | 140 - 180 °C | 284 - 356 °F | Injection molding |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Mold Temperature | 140 - 230 °C | 284 - 446 °F | short vulcanization time required (a few seconds) |
Momentive Performance Materials Silopren™ LSR 3386/30 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Mold Temperature | 140 - 160 °C | 284 - 320 °F | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |