Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 93.3 - 149 °C | 200 - 300 °F | |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Mold Temperature | 93.3 - 110 °C | 200 - 230 °F | |
Polymer Resources NY66-G20-MD Nylon 66, 20% Glass Reinforced with MoS2 Nylon 66, 20% Glass Reinforced with Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigment.. |
|||
Mold Temperature | 93.3 - 110 °C | 200 - 230 °F | |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Mold Temperature | 93.3 - 149 °C | 200 - 300 °F | |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Mold Temperature | 93.3 - 107 °C | 200 - 225 °F | |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Edgetek® PS-20GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(dis Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Mold Temperature | 93.3 - 149 °C | 200 - 300 °F | |
PolyOne Edgetek® RA-20CF/000 Polyarylsulfone, Carbon Fiber Reinforced
(discontinued **) Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 93.3 - 121 °C | 200 - 250 °F | |
Clariant Renol BR2084 Nylon 66, 33% Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Mold Temperature | 93.3 °C | 200 °F | |
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla.. |
|||
Mold Temperature | 93.3 - 163 °C | 200 - 325 °F | |
PolyOne Lubri-Tech™ RA-15GF/13T Polyethersulfone, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |