Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 277 - 299 °C | 530 - 570 °F | |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Nozzle Temperature | 277 - 299 °C | 530 - 570 °F | |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Nozzle Temperature | 160 - 299 °C | 320 - 570 °F | Average value: 199 °C Grade Count:75 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Nozzle Temperature | 271 - 299 °C | 520 - 570 °F | reverse tapered recommended |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 277 - 299 °C | 530 - 570 °F | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 179 - 299 °C | 354 - 570 °F | Injection |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Nozzle Temperature | 277 - 299 °C | 530 - 570 °F | |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Nozzle Temperature | 266 - 299 °C | 510 - 570 °F | |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 277 - 299 °C | 530 - 570 °F | |
Entec Hylex® P1010FR Polycarbonate Information provided by Ravago. |