Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Nozzle Temperature | 193 - 210 °C | 379 - 410 °F | |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Nozzle Temperature | 193 - 224 °C | 379 - 435 °F | |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Nozzle Temperature | 193 - 224 °C | 379 - 435 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Nozzle Temperature | 193 - 224 °C | 379 - 435 °F | |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ OM 1255NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1255NX-9 is a performance TPU alloy designed for thin wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Improved Grip with Matte, Rubbery Finish - Superior Adhesi.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 °C | 379 °F | Typical die temp for tube extrusion. |
DuPont 20 Series 2020 Specialty Polyethylene Resin
(discontinued **) DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7690-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Nozzle Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Nozzle Temperature | 193 - 227 °C | 379 - 441 °F | |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 °C | 379 °F | Typical die temp for tube extrusion. |
DuPont 20 Series 2020T Specialty Polyethylene Resin DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |