Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 285 - 305 °C | 545 - 581 °F | Injection Molding |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
Nozzle Temperature | 285 - 305 °C | 545 - 581 °F | Injection Molding |
LG Chemical LUPOY SC1004A PC Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information.. |
|||
Nozzle Temperature | 285 - 305 °C | 545 - 581 °F | Injection Molding |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Nozzle Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 290 - 305 °C | 554 - 581 °F | Injection Molding |
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
Nozzle Temperature | 285 - 305 °C | 545 - 581 °F | Injection Molding |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Nozzle Temperature | 280 - 305 °C | 536 - 581 °F | |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Nozzle Temperature | 230 - 305 °C | 446 - 581 °F | Average value: 279 °C Grade Count:10 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Nozzle Temperature | 285 - 305 °C | 545 - 581 °F | Injection Molding |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |