Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4003 Anhydride-Modified HDPE Adhesive Resin
(discontinued **) Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 11E573 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3062 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Nozzle Temperature | 235 - 280 °C | 455 - 536 °F | Average value: 263 °C Grade Count:3 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Nozzle Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9255D Ester Type TPE Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Nozzle Temperature | 235 - 270 °C | 455 - 518 °F | Injection Molding |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Nozzle Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 4001 LC Black TPE Thermoplastic Elastomer Features: Heat Resistance, HighOzone ResistantCompression Set, Low Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F.. |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® D 3804 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 40E529 Anhydride-Modified HDPE Adhesive Resin Bynel® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 1123 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Nozzle Temperature | 235 °C | 455 °F | Die |
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Nozzle Temperature | 235 - 240 °C | 455 - 464 °F | |
Beijing Chemical Industry KAIFA® HN201-G0 PA6 Resin Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 235 °C | 455 °F | |
Multibase Multi-Flex® A 6221 CUV A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |