Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
RheTech Products HP520-00 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Average value: 220 °C Grade Count:26 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
LG Chemical LI921NS ASA Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3300 PP+MF30% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5157Z PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good PaintabilityApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS GP-2106F General Purpose ABS, 10% Glass Fiber Reinforced, Weather Resistant, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 210 °C | 410 °F | |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF3308C PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Che.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5150H PP+MF15%, High Flow Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5204B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL LW4405 PP+GF/MF40% Description: Injection Molding, PP+GF/MF40%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 65997-17-3 and 12001-26-2Information provided by LG Chemical |
|||
Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical LUPOL MC4352 PP+Rubber+MF Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9.. |
|||
Nozzle Temperature | 210 °C | 410 °F | Recommended |
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 210 - 260 °C | 410 - 500 °F | Average value: 218 °C Grade Count:24 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |