Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 324 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:..
Front Barrel Temperature 324 - 340 °C
615 - 644 °F
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)  (discontinued **)
Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural..
Front Barrel Temperature 324 °C
615 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better ..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)  (Unverified Data**)
Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber
Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber
Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Front Barrel Temperature 324 - 340 °C
615 - 644 °F
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Front Barrel Temperature 324 - 340 °C
615 - 644 °F
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep ..
Front Barrel Temperature 324 °C
615 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Front Barrel Temperature 324 °C
615 °F
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
Front Barrel Temperature 324 - 345 °C
615 - 653 °F
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber
Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber
Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)  (Unverified Data**)
Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of ..
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers.
Copyright © lookpolymers.com All Rights Reserved