Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon .. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Star Plastics PC741 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Entec Hylex® P1010FR Polycarbonate Information provided by Ravago. |