Polymer Property : Middle Barrel Temperature = 320 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement  (discontinu
Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu..
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral  (discontinued **)
Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu..
Middle Barrel Temperature 270 - 320 °C
518 - 608 °F
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Injection Molding
LG Chemical LUCON CP510F PC/ABS+CNT
Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b..
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Injection Molding
LG Chemical LUCON PN9008 PPS+MF+GF
Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212..
Middle Barrel Temperature 310 - 320 °C
590 - 608 °F
Injection Molding
LG Chemical LUCON PN9009 PPS+MF
Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2..
Middle Barrel Temperature 270 - 320 °C
518 - 608 °F
Injection Molding
LG Chemical LUCON SP9306FL sPS+MF
Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 ..
Middle Barrel Temperature 300 - 320 °C
572 - 608 °F
Unitika P-5001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
Middle Barrel Temperature 270 - 320 °C
518 - 608 °F
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..