Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 263 - 274 °C | 505 - 525 °F | |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Middle Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
Middle Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 263 - 268 °C | 505 - 515 °F | |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 263 - 274 °C | 505 - 525 °F | |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |