Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Middle Barrel Temperature | 243 - 266 °C | 469 - 511 °F | |
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-FR1 PBT, 30% Glass Reinforced Structural Foam Grade, Flame Retardant Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 469 - 500 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Middle Barrel Temperature | 243 - 254 °C | 470 - 490 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 243 °C | 470 °F | |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |
|||
Middle Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |