Polymer Property : Cure Time = 0.167 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Cure Time 5.00 - 10.0 min

@Temperature 150 °C
0.0833 - 0.167 hour

@Temperature 302 °F
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Cure Time 5.00 - 10.0 min

@Temperature 120 °C
0.0833 - 0.167 hour

@Temperature 248 °F
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..
Cure Time 8.00 - 10.0 min

@Temperature 100 °C
0.133 - 0.167 hour

@Temperature 212 °F
Lord Adhesives Thermosetâ„¢ SC-102 Unfilled Silicone Encapsulant
Lord SC-102 is a "water-white" clear, two component, silicone encapsulating system. It has a very low viscosity and, when cured, a low Shore A hardness. Lord SC-102 is optically transparent with no ..
Cure Time 4.98 - 10.0 min

@Temperature 149 °C
0.0830 - 0.167 hour

@Temperature 300 °F
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive
Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt..
Cure Time 4.98 - 10.0 min

@Temperature 149 °C
0.0830 - 0.167 hour

@Temperature 300 °F
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive
Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic..
Cure Time 7.98 - 10.0 min

@Temperature 75.0 °C
0.133 - 0.167 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Blue River Coatings Acrylic 4000D Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..
Cure Time 7.98 - 10.0 min

@Temperature 75.0 °C
0.133 - 0.167 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Blue River Coatings Acrylic 4000 Topcoat
BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo..