Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 27.6 - 51.7 MPa | 4000 - 7500 psi | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |