Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black
Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural
Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural
Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural
Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural
Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black
Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Hold Pressure 27.6 - 51.7 MPa
4000 - 7500 psi
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved