Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F38-04 35% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, White Applications: HousingsBracketsSupport ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F43-01A 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical component supportsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1001-74 Thermoplastic Polyolefin, Non-UV Stabilized, DX9 Black Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products HP522-390 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, AYCA Medium Prairie Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products M30P100-01 30% Mica Reinforced Polypropylene, Black Applications: Fan shroudsHVAC ductworkClose-out panelsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products P258-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Door/trunk scuffExterior grills and cowlsSteering column shroudsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products T40P100-00A 40% Talc Reinforced Polypropylene, Natural Applications: Durable goodsHVAC componentsFunctional supportsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Hold Pressure | 2.07 - 8.27 MPa | 300 - 1200 psi | |
RheTech Products GC20P100-00UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |