Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Zone 3 | 240 °C | 464 °F | Injection Molding |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Zone 3 | 240 °C | 464 °F | Injection Molding |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide P1000IX1 PA6, Impact Modified, Injection Molded Staramide P1000IX1 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI006 or Star X 2006)Information provided by Eurostar. |
|||
Zone 3 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 °C | 464 °F | |
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starpylen MX05038 TPEX, Injection Molded Starpylen MX05038 is a TPEX Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Star L PA6 D61 PA6, Injection Molded Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 °C | 464 °F | Metering-zone |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |