Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 165 - 180 °C
329 - 356 °F
Injection Molding
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound
Zone 2 170 - 180 °C
338 - 356 °F
Extrusion Molding
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound
Zone 2 170 - 180 °C
338 - 356 °F
Extrusion Molding
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry Parts Information provided by API-Kolon.
Zone 2 170 - 180 °C
338 - 356 °F
Extrusion Molding
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Zone 2 170 - 180 °C
338 - 356 °F
Injection Molding
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Zone 2 170 - 180 °C
338 - 356 °F
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEM”; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki..
Copyright © lookpolymers.com All Rights Reserved