Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 302 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin
Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin
Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin
Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin
Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or ..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin
Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/4 Polyolefin
Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin
Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st..
Zone 2 150 - 165 °C
302 - 329 °F
Solvay Specialty Polymers Cogegum® GFR/320 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Polidan® EC/MD Polyethylene, Crosslinked (XLPE)
Medium density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes...
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE)
POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 2 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 2 150 °C
302 °F
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable
Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D867 Ethylene Acrylate
DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Zone 2 150 °C
302 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Zone 2 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou..