Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Die Temperature | 170 - 220 °C | 338 - 428 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1134 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1134 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BB108E Polypropylene compound for Steel Pipe Coating BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coa.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BEC5015 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BEC5015 is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength.BorECO BEC5015 is recommended for solid wall and structured wall n.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BS4641 High Density Polyethylene BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6020 Polypropylene Random Copolymer RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Average value: 205 °C Grade Count:18 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Die Temperature | 182 - 220 °C | 360 - 428 °F | Average value: 204 °C Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |