Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
|
Victrex® HT™ P22 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850/CF/10/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-8106 Polyacetal-copolymer, with carbon fiber, PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7709/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Drying Temperature | 120 °C @Time 14400 - 21600 sec |
248 °F @Time 4.00 - 6.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Drying Temperature | 120 °C @Time 7200 - 14400 sec |
248 °F @Time 2.00 - 4.00 hour |
Air-Circulation Dryer |
Lehmann & Voss LUVOCOM® 80-8072 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Drying Temperature | 120 °C @Time 21600 - 28800 sec |
248 °F @Time 6.00 - 8.00 hour |
or |
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Drying Temperature | 120 °C @Time 21600 sec |
248 °F @Time 6.00 hour |
Horizontal Oven |
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6 Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 120 °C @Time 14400 sec |
248 °F @Time 4.00 hour |
Chute Hot-Wind |
Zhejiang Juner PC-A2-10 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Drying Temperature | 120 °C @Time >=28800 sec |
248 °F @Time >=8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |