Polymer Property : Drying Temperature = 176 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 19-7319 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..
Drying Temperature 80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 80.0 °C

@Time 7200 - 28800 sec
176 °F

@Time 2.00 - 8.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Drying Temperature 80.0 °C

@Time 21600 - 57600 sec
176 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Drying Temperature 80.0 °C

@Time 21600 - 57600 sec
176 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 57600 sec
176 °F

@Time 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Drying Temperature 80.0 °C

@Time 57600 sec
176 °F

@Time 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Drying Temperature 80.0 °C

@Time 57600 sec
176 °F

@Time 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Drying Temperature 80.0 °C

@Time 57600 sec
176 °F

@Time 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop..
Drying Temperature 80.0 °C

@Time 21600 - 57600 sec
176 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Drying Temperature 80.0 °C

@Time 21600 - 57600 sec
176 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Drying Temperature 80.0 °C

@Time 21600 - 28800 sec
176 °F

@Time 6.00 - 8.00 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Drying Temperature 80.0 °C

@Time 7200 - 43200 sec
176 °F

@Time 2.00 - 12.0 hour
Vacuum Dryer
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te..