Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Hardening Temperature |
Möller Medical PolySkin 82 NanoCoating Flexible, very non-abrasive, chemical-resistant decorative coating.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1410 Polyolefin TPO Granules, Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Membranes |
Lucobit Lucofin® 1411-t1 Polyolefin TPO Granules, White Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1412 Polyolefin TPO Granules, Light Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1459 Polyolefin TPO Granules, Azure Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | |
Taiwan Sheen Soon Sheenthane® A8631N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | |
Taiwan Sheen Soon Sheenthane® A8820N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Lamination Adhesive |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
Fainplast Compounds Hax™ HF 045/16M Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, low shrinkageInformation provided by Fainplast Compounds |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucobit® 1235 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of special.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1410MB Polyolefin TPO Granules, Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1460 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |