Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Plasticizing Zone |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Processing Temperature | 135 - 155 °C | 275 - 311 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Processing Temperature | 135 - 160 °C | 275 - 320 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Injection moulding, matched metal die |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Processing Temperature | 135 - 150 °C | 275 - 302 °F | Compression moulding, matched metal die |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Processing Temperature | 135 °C | 275 °F | Normal Forming Temperature |
Spartech Polypedic Modified Low Density Polyethylene Description: Flexible, wider window for forming, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOs; prosthetic flexible socketsInformation provided by.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 0.5-1 hr. |
Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 3 hr. |
Von Roll Isola IMI Varnish 3255 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Processing Temperature | 135 °C | 275 °F | Suggested baking time at this temperature is 6-18 hr. May also be cured for shorter time at higher temperatures. |
Von Roll Isola IMI E-Solder® 3012 Electrically Conductive Adhesive Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t.. |
|||
Processing Temperature | 135 °C | 275 °F | Cure Temp |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Processing Temperature | 135 - 180 °C | 275 - 356 °F | Average value: 162 °C Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 135 - 293 °C | 275 - 560 °F | Average value: 263 °C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Processing Temperature | 135 - 165 °C | 275 - 329 °F | Molding temperature |
Cosmic Plastics CP7314 Epoxy Molding Compound Data provided by the manufacturer. |