Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation

Category Polymer , Thermoset , Epoxy , Solventless Epoxy Varnish, Electrical Insulation
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Von Roll Isola USA.Flash Point: 19°C. Average solids: 60%. Usage Notes: Use with IMI 74010 hardener for final coat over field coils, windings, and heavy duty motors.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Viscosity <= 50 cP
<= 50 cP
Hardener
170 cP
170 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Electrical Properties Metric English Comments
Dielectric Strength 39.0 kV/mm
991 kV/in
Processing Properties Metric English Comments
Processing Temperature 135 °C
275 °F
Suggested baking time at this temperature is 0.5-1 hr.