Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 290 - 310 °C | 554 - 590 °F | |
PolyChem Alloy PolyFast 8167UC UV Stabilizer Masterbatches For Nylon |
|||
Processing Temperature | 191 - 310 °C | 376 - 590 °F | Average value: 262 °C Grade Count:13 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Processing Temperature | 249 - 310 °C | 480 - 590 °F | Average value: 291 °C Grade Count:43 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Processing Temperature | 204 - 310 °C | 399 - 590 °F | Injection |
Dyna-Purge® C Purging Compound Designed for Purging Transparent ResinsGeneral Description:DYNA-PURGE C is a clear, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to purge high clarity.. |
|||
Processing Temperature | 204 - 310 °C | 399 - 590 °F | Extrusion |
Dyna-Purge® C Purging Compound Designed for Purging Transparent ResinsGeneral Description:DYNA-PURGE C is a clear, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to purge high clarity.. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM 45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | Injection |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | Melt |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Processing Temperature | 250 - 310 °C | 482 - 590 °F | Resin Temperature |
Asahi Kasei Xyron® 600H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | Average value: 293 °C Grade Count:3 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |