Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 221 - 290 °C | 430 - 554 °F | Average value: 263 °C Grade Count:22 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A5 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A7-5 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Ter Hell Plastic Terez® PA 6.6 7750 T Polyamide 66 Description: Dry impact unfilled Polyamide 6.6, good flowability and demolding properties.Application: Molding parts of different kinds, high impact properties.Information provided by Ter Hell Plas.. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TB120SG30 Impact Modified, 30% Glass Fiber Reinforced PA6, DAM 30% Glass Fiber reinforced, High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT70 GR15 NL100 MB PET, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 PR PET, 30% glass fiber reinforced, high heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT74 CR20 BK111 PR PET, 20% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TA210 LW TA210LW, Low Wear, Low Friction PA66, DAM Low wear, Low frictionInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | Extrusion |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Processing Temperature | 240 - 290 °C | 464 - 554 °F | Resin Temperature |
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A1-1 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A1-11 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A1-3 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 290 °C | 482 - 554 °F | |
Zhejiang Juner PC-A1-7 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 260 - 290 °C | 500 - 554 °F | Resin Temperature |
Asahi Kasei Xyron® X5403 PPE/PA Oil ResistantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 290 °C | 428 - 554 °F | |
E-Polymers Tekaloy® G70A2 Impact Resistance, Easy Molding PC/ABS Alloy Impact Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd. |