Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 21.1 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPC-W44A Polyurethane Gel
MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPL-R20B Rigid Polyurethane Foam Formulation
This rigid polyurethane foam system is one of a family of polymer systems developed by Northstar Polymers for specific applications. Urethane foams molded with this system exhibit closed cell struct..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-A50A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-A90A High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 25.0 °C
70.0 - 77.0 °F
Prepolymer Temperature
Northstar Polymers MPP-D65A Polyether Base Polyurethane Resin
MPP-D65A is a polyether base 2-component polyurethane resin casting system for molding and potting applications. It has a long pot-life and gradual curing pattern to provide easier handling for mol..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-D80B Rigid Polyurethane
MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus..
Processing Temperature 21.1 - 29.4 °C
70.0 - 85.0 °F
Curing Agent Temperature
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation
MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-R02C Semi-rigid Polyurethane Foam Formulation
MPP-R02C is semi-rigid foam formulations for molded foam products. It is closed-cell light foam with some structural integrity. Unlike rigid polyurethane foams, the physical properties of a cured pr..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-R07B Polyurethane Formulation
This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is long enough to allow manual handling for cast-..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPS-F04A Hand-Mixable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPS-F06B Hand-Mixable Flexible Foam
This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing or by the meter dispensing equipment. The components are stable liquid at room temperature and..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane
This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste..
Processing Temperature 21.1 °C
70.0 °F
Prepolymer Temperature
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers VEF-41 Viscoelastic Foam Formulation
Viscoelastic foam has a very unique recovery property and very low compression deflection property. When the foam is compressed by a hand it can leave imprint of the hand, and then it slowly recove..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MAP-R06C Semi Rigid Structural Foam Formulation
MPP-R06C is a polyurethane foam formulation. It is closed-cell foam with a good structural integrity and an enhanced skin quality. Unlike polyurethane rigid foams, the physical properties of a cured..
Processing Temperature 21.1 - 25.0 °C
70.0 - 77.0 °F
Curing Agent Temperature
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Prepolymer Temperature
Northstar Polymers MPP-A80E High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPP-A80E High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers MPS-M23B Room-Temperature Curable Microcellular Foam
This foam polyurethane formulation is designed to yield closed-cell microcellular foam by either hand-mixing or machine casting method at room temperature. The components are liquid at room temperat..
Processing Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Curing Agent Temperature
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the ..
Processing Temperature 21.1 °C
70.0 °F
Devcon Backing Compound Epoxy
Abrasion-Resistant SystemData provided by Ellsworth Adhesives.
Processing Temperature 21.1 °C
70.0 °F
Devcon Brushable Ceramic - White Epoxy
Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,..
Processing Temperature 21.1 °C
70.0 °F
Devcon Carbide Putty Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Processing Temperature 21.1 °C
70.0 °F
Devcon High-Performance Backing Compound Epoxy
Abrasion-Resistant SystemData provided by Ellsworth Adhesives.
Processing Temperature 21.1 °C
70.0 °F
Devcon Sprayable Ceramic™ Epoxy
Precision Repair EpoxyComments: A sprayable ceramic-reinforced composite that can be sprayed in a manner similar to high-solid paints. Ideal for protecting pumps, paper machines, stacks, pump pads,..
Processing Temperature 21.1 °C
70.0 °F
Devcon Tile Adhesive Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Processing Temperature 21.1 °C
70.0 °F
Devcon Wear Guard (Fine Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Processing Temperature 21.1 °C
70.0 °F
Devcon Wear Guard (High Temp) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Processing Temperature 21.1 - 60.0 °C
70.0 - 140 °F
Average value: 28.9 °C Grade Count:14
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..
Copyright © lookpolymers.com All Rights Reserved