Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for this formulation includes prototyping, casing, and in-house tool making. The components for this formulation have low viscosity, which is an advantage to fill thinner parts of the mold; it helps recreating the fine resolution of the mold surface pattern, and avoids trapping large air bubbles. Relatively forgiving pot-life and short demolding time helps the production rate when it is use in a project with a larger production quantity requirement.Information provided by Northstar Polymers.
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 70
65 - 70
ASTM D2240
Tensile Strength 24.8 MPa
3600 psi
ASTM D412
Elongation at Break 60 %
60 %
ASTM D412
Tear Strength 154 kN/m
880 pli
Die C; ASTM D624
Processing Properties Metric English Comments
Processing Temperature 21.1 - 25.0 °C
70.0 - 77.0 °F
Prepolymer Temperature
21.1 - 25.0 °C
70.0 - 77.0 °F
Curing Agent Temperature
Mold Temperature 21.1 - 48.9 °C
70.0 - 120 °F
Cure Time 6.00 - 42.0 min

@Temperature 25.0 °C
0.100 - 0.700 hour

@Temperature 77.0 °F
De-mold Time
4320 - 10100 min

@Temperature 25.0 °C
72.0 - 168 hour

@Temperature 77.0 °F
Complete Cure Cycle
Pot Life 3.00 min
3.00 min
Descriptive Properties Value Comments
Curing Agent PBA-013
Prepolymer MGA-018
Weight Ratio 1:0.675
Prepolymer to Curing Agent Ratio
Users viewing this material also viewed the following: