Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 193 - 210 °C | 380 - 410 °F | Profile |
S&E Specialty Polymers TufFill™ 5000-SN4 PP, Flame Retardant Application: A No Bloom, UL 94 V-0 Polypropylene Compound TufFill™ 5000SN series is a specially engineered, low bloom, flame retardant polypropylene compound designed with halogen based technology... |
|||
Processing Temperature | 193 - 210 °C | 379 - 410 °F | Optimum Extrusion Temperature |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Processing Temperature | 193 - 232 °C | 380 - 450 °F | Average value: 214 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Processing Temperature | 193 - 232 °C | 380 - 450 °F | Average value: 215 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Processing Temperature | 193 - 221 °C | 379 - 430 °F | Blow Molding |
Chevron Phillips Marlex® C579 High density polyethylene
(discontinued **) Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceApplications: multi-layer fuel tanks, mono-layer fuel tanks, industrial bulk containersInformation pro.. |
|||
Processing Temperature | 193 - 216 °C | 379 - 421 °F | Stock Temperature |
Chevron Phillips Marlex® HHM TR-144 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Processing Temperature | 193 - 232 °C | 379 - 450 °F | Stock Temperature |
Chevron Phillips Marlex® HHM TR-166 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Processing Temperature | 193 - 210 °C | 379 - 410 °F | stock temperature |
Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer
(discontinued **) Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: pond liners, gas and chemical tank containment liners, landfill liner.. |
|||
Processing Temperature | 193 - 216 °C | 379 - 421 °F | adequate mixing to achieve good dispersion |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:8 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:3 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:7 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:7 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Processing Temperature | 193 - 221 °C | 379 - 430 °F | Extrusion |
Shuman 210 Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Processing Temperature | 193 - 221 °C | 379 - 430 °F | Extrusion |
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Processing Temperature | 193 - 210 °C | 379 - 410 °F | stock temperature |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
Processing Temperature | 193 - 216 °C | 379 - 421 °F | Stock |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Processing Temperature | 193 - 210 °C | 379 - 410 °F | stock temperature |
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust.. |
|||
Processing Temperature | 193 - 232 °C | 379 - 450 °F | Extrusion |
Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer Fully Formulated Medium Density Hexene CopolymerCustomer Benefits: This extrusion grade hexene copolymer has good processability, excellent melt strength, broad fusion range, outstanding ESCR, meets.. |
|||
Processing Temperature | 193 - 232 °C | 379 - 450 °F | Extrusion |
Chevron Phillips Marlex® K606 High Density Polyethylene High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to.. |
|||
Processing Temperature | 193 °C | 379 °F | Film extrusion temperature |
Dow LDPE 609A Low Density Polyethylene, High Clarity Film Grade DOW LDPE 609A resin is a fully formulated high strength clarity film resin for optical packaging applications, such as produce and bakery film. It contains medium levels of slip additive and low lev.. |
|||
Processing Temperature | 193 - 232 °C | 379 - 450 °F | Extrusion |
Chevron Phillips Marlex® K607 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to.. |
|||
Processing Temperature | 193 - 249 °C | 380 - 480 °F | Average value: 222 °C Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Processing Temperature | 193 - 240 °C | 380 - 464 °F | Average value: 211 °C Grade Count:7 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:5 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Processing Temperature | 193 - 227 °C | 380 - 440 °F | Average value: 210 °C Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |