Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 150 - 210 °C | 302 - 410 °F | |
PolyChem Alloy GMS 2004D Foam Stabilizer PE Foam Stabilizer |
|||
Processing Temperature | 150 °C | 302 °F | Compression or Injection Molding |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression or Injection Molding |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Processing Temperature | 150 °C | 302 °F | Injection or Compression Molding |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression Molding |
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Processing Temperature | 150 °C | 302 °F | Injection or Compression Molding |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Processing Temperature | 150 °C | 302 °F | Compression or Injection Molding |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Average value: 166 °C Grade Count:5 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1411 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1412 Polyolefin TPO Granules, Light Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 150 - 180 °C | 302 - 356 °F | Profiles |
Lucobit Lucofin® 1414 Polyolefin TPO Granules, Silk Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucolit® 1321 Polyolefin TPO Granules, Blue Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucofin® 1414-t2 Polyolefin TPO Granules, Silk Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t2 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | |
Taiwan Sheen Soon Sheenthane® A8600F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 150 °C | 302 °F | Suggested baking time at this temperature is 4-6 hr. |
Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 50%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, bare copper coils, etc.. |
|||
Processing Temperature | 150 - 175 °C | 302 - 347 °F | Molding temperature |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Processing Temperature | 150 - 175 °C | 302 - 347 °F | Molding temperature |
Cosmic Plastics E4930 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Processing Temperature | 150 - 170 °C | 302 - 338 °F | |
Wanhua Chemical Wanthane® WHT-1680AB Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 150 °C | 302 °F | Cure 0.25 hrs |
Aptek 2710A/B Low modulus silicone adhesive Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)APTEK 2710-A/B is a two component, black, low modulus, thixotropic, s.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Coating Temperature |
BACT Dylyn® Diamond-Like Nanocomposite Coating a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Coating Temperature |
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating Metal-doped Me/a-C:H/a-Si:O nanocomposite. The electrical characteristics of these coatings can be tailored by the addition of metal dopants. This creates an engineered surface for specialized ap.. |
|||
Processing Temperature | 150 - 175 °C | 302 - 347 °F | Average value: 163 °C Grade Count:3 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Processing Temperature | 150 - 200 °C | 302 - 392 °F | Profiles |
Lucobit Lucolit® 1320 Polyolefin TPO Granules, Beige Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 150 °C | 302 °F | Press Cure, 8-10 minutes |
Mitsui MILEX™ Straight Novolak Phenolic Resin
(discontinued **) The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic .. |