Mitsui MILEX™ Straight Novolak Phenolic Resin  (discontinued **)

Category Polymer , Thermoset , Phenolic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mitsui MILEX™ Straight Novolak Phenolic Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The MILEX™ Family of products is widely featured in brake systems of automobiles made by the top automakers through Mitsui Chemicals' affiliation with leading brake manufacturers. The phenolic material is primarily used as binders in brake pad and clutch facing disc friction materials. The advantage of incorporating the MILEX material into a brake design is that the material provides a non-abrasive, vibratory free surface finish, which is very important in the performance of the brake system. Additionally, its superior performance at elevated temperatures and excellent moldability aids in brake noise reduction.Applications: Automotive friction materials (brake pads, clutch facing discs, etc)Epoxy resin hardener for electronic materialsAdditive to improve heat resistance of thermoplasticsAdhesives, especially with elastomers, to bond to metalInformation provided by Mitsui.
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Press Cure, 8-10 minutes
180 °C
356 °F
Post cure, 5 hours
Descriptive Properties Value Comments
Cracking Resistance 1
5=Excellent
Curing Rate 5
1=Slow, 5=Fast
Hardness 1
1=Hard, 5=Soft
Heat Resistance 2
1-5 (5-Excellent)