Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 96.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX AS002 ABS
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66  (Unverified Data**)
Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific)
LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopolymer
LNP* LUBRICOMP* KP003AXZ is a compound based on Acetal Homopolymer resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66
LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific)
LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 0.000 - 100 °C
53.3 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM E228
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
53.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
Copyright © lookpolymers.com All Rights Reserved