Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 55.0 - 160 °C |
52.8 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN53G50HSLR BK083 is a 50% glass reinforced, heat stabilized, lubricated high performance polyamide resin developed for moderate temperature structural applications requiring retention of h.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 100 - 200 °C |
52.8 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
52.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Asia Pacific) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
52.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 150 °C |
52.8 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East) Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific) LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |