Polymer Property : CTE, linear, Transverse to Flow = 130 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWE265 ASA
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 40.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East)
Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® FG6129 NC010 PBT  (Unverified Data**)
Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 150 - 250 °C
72.2 µin/in-°F

@Temperature 302 - 482 °F
ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 150 - 200 °C
72.2 µin/in-°F

@Temperature 302 - 392 °F
ASTM E831
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 160 - 249 °C
72.2 µin/in-°F

@Temperature 320 - 480 °F
ASTM E831
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 100 °C
72.2 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer  (Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 100 - 250 °C
72.2 µin/in-°F

@Temperature 212 - 482 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA), 22% Glass Fiber
Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material ..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 150 - 200 °C
72.2 µin/in-°F

@Temperature 302 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 150 - 200 °C
72.2 µin/in-°F

@Temperature 302 - 392 °F
TMA; ASTM E831
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 23.0 - 80.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 95.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 95.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 95.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature -40.0 - 95.0 °C
72.2 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66  (Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66  (Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66  (Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 160 °C
72.2 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66  (Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 120 °C
72.2 µin/in-°F

@Temperature 131 - 248 °F
ASTM E 831
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET  (Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 120 °C
72.2 µin/in-°F

@Temperature 131 - 248 °F
ISO 11359-1/-2
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET  (Unverified Data**)
Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon..
CTE, linear, Transverse to Flow 130 µm/m-°C

@Temperature 55.0 - 100 °C
72.2 µin/in-°F

@Temperature 131 - 212 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform..