Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature 23.0 - 55.0 °C |
62.8 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature 23.0 - 55.0 °C |
62.8 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific) LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific) LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br.. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific) LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp SF006S PA 12 LNP* Thermocomp* SF006S is a compound based on Nylon 12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re.. |
|||
CTE, linear, Transverse to Flow | 113 µm/m-°C @Temperature 23.0 - 55.0 °C |
62.8 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |