Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 40.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 30.0 - 100 °C |
66.7 µin/in-°F @Temperature 86.0 - 212 °F |
|
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 30.0 - 100 °C |
66.7 µin/in-°F @Temperature 86.0 - 212 °F |
|
3M Dyneon™ 1502 PTFE Powder
(discontinued **) Type VI PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 30.0 - 300 °C |
66.7 µin/in-°F @Temperature 86.0 - 572 °F |
|
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 30.0 - 200 °C |
66.7 µin/in-°F @Temperature 86.0 - 392 °F |
|
3M Dyneon™ TF 4303 PTFE 15% Graphite Filled
(discontinued **) Type II PTFE. Applications include sliding surfaces, bearings, seals/gaskets.Data provided by Dyneon. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS) Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 100 - 200 °C |
66.7 µin/in-°F @Temperature 212 - 392 °F |
2 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -30.0 - 30.0 °C |
66.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 23.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature -40.0 - 23.0 °C |
66.7 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
CTE, linear, Parallel to Flow | 120 µm/m-°C @Temperature >=143 °C |
66.7 µin/in-°F @Temperature >=289 °F |
Above Tg; ISO 11359 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |